Response surface analysis of removal of a textile dye by a Turkish coal powder
Özet
In the present study, an experimental design methodology was used to optimize the adsorptive removal of Basic Yellow 13 (BY13) using Turkish coal powder. A central composite design (CCD) consisting of 31 experiments was employed to evaluate the simple and combined effects of the four independent variables, initial dye concentration (mg/L), adsorbent dosage (g/L), temperature (inverted perpendicular C) and contact time (min) on the color removal (CR) efficiency (%) and optimizing the process response. Analysis of variance (ANOVA) showed a high coefficient of determination value (R-2 = 0.947) and satisfactory prediction of the polynomial regression model was derived. Results indicated that the CR efficiency was not significantly affected by temperature in the range of 12- 60 degrees C. While all other variables significantly influenced response. The highest CR (95.14%), estimated by multivariate experimental design, was found at the optimal experimental conditions of initial dye concentration 30 mg/L, adsorbent dosage 1.5 g/L, temperature 25 degrees C and contact time 10 min.
Anahtar kelimeler
Sürdürülebilir Kalkınma Amaçları
-
SKA 12: Sorumlu Üretim ve Tüketim
Atıf için künye
KHATAEE, A. R., Alidokht, L., Hassani, A., & Karaca, S. (2013). Response surface analysis of removal of a textile dye by a Turkish coal powder. ADVANCES IN ENVIRONMENTAL RESEARCH-AN INTERNATIONAL JOURNAL, 2(4), 291–308. https://doi.org/10.12989/aer.2013.2.4.291
BibTeX
@article{khataee2013-69561,
author = {KHATAEE, A. R. and Alidokht, Leila and Hassani, Aydin and Karaca, Semra},
title = {Response surface analysis of removal of a textile dye by a Turkish coal powder},
journal = {ADVANCES IN ENVIRONMENTAL RESEARCH-AN INTERNATIONAL JOURNAL},
year = {2013},
volume = {2},
number = {4},
pages = {291--308},
issn = {2234-1722},
doi = {10.12989/aer.2013.2.4.291},
url = {https://akademik.atauni.edu.tr/yayinlar/69561-response-surface-analysis-of-removal-of-a-textile-dye-by-a-turkish-coal-powder}
}