Effect of pH on the Stress Corrosion Cracking ofAZ91 Mg Alloys Using Slow Strain Rate Test(SSRT) Method
International Conference on Advances and Innovations in Engineering (ICAIE)
ss. 542–546 · Elazığ · 10.05.2017–12.05.2017 · 10.05.2017
Atıf için künye
ÇATAR, R., & Altun, H. (2017). Effect of pH on the Stress Corrosion Cracking ofAZ91 Mg Alloys Using Slow Strain Rate Test(SSRT) Method. International Conference on Advances and Innovations in Engineering (ICAIE), Elazığ (ss. 542–546).