Wear properties of plasma nitrided Inconel 718 superalloy
13th International Conference on Plasma Surface Engineering-PSE
Garmisch-Partenkirchen · 10.09.2012–14.09.2012 · 10.09.2012
Atıf için künye
Kovacı, H., ASL GHAHRAMANZADEH, H., ALBAYRAK, Ç., & ALSARAN, A. (2012). Wear properties of plasma nitrided Inconel 718 superalloy. 13th International Conference on Plasma Surface Engineering-PSE, Garmisch-Partenkirchen.